Ana Sofia Figueira Ramos is Assistant Professor at the Department of Mechanical Engineering (DEM) of the Faculty of Sciences and Technology of the University of Coimbra (FCTUC), since September 2019. She belongs to the Centre for Mechanical Engineering, Materials and Processes - CEMMPRE. A.S. Ramos completed her 5 year degree in Chemical Engineering by the University of Coimbra (UC) in 1994 . In 1997 she finished the MSc in Materials Engineering and in 2002 she completed a PhD in Mechanical Engineering with full honour (MSc and PhD FCT studentship).
Loading... 3 0 20 0 false

Publications
(All)

Refined By:
Author:  Morgiel, Jerzy
Subject:  sputtering
Subject:  nanoindentation

Results 1-1 of 1 (Search time: 0.002 seconds).

Issue DateTitleAuthor(s)TypeAccess
12020Effect of Deposition Parameters on the Reactivity of Al/Ni Multilayer Thin FilmsRamos, Ana Sofia ; Simões, Sónia; Maj, Lukasz; Morgiel, Jerzy; Vieira, Maria Teresa articleopenAccess